OIL FREE SATURATED POLYESTER RESIN Type :  Oil free saturated polyester resin
Type :  Oil free saturated polyester resin
      Form of delivery: 65 % in solvent C-9/ Butyl glycol (4:1)
General Information :
KP – 5065 is linear oil free polyester super durable resin developed for use in coil coating, sheet fed
        metal decorating and general industrial applications. KP-5065 is engineered for high performance and
        good exterior durability and high performance.
Features :
KP-6065 is engineered for severe exterior building product applications. High weatherability, Good
        formability, Excellent weathering performance, materials for buildings.
| 1. Appearance | : | Clear transparent viscous liquid | 
| 2. Colour | : | Pale yellow to water white | 
| 3. Acid value (mg.KOH/gm.) | : | 0-5 Max. | 
| 4. Non volatile matter ( 1 hr @ 150 ºC | : | 65 ± 2 % | 
| 5. Viscosity @25 ºC (4/20 RPM) B.Field | : | 3500 -40000 Cps | 
| 6. Hydroxyl value | : | 40 – 45 mgKOH/g | 
| 7. Specific gravity | : | 1.08 ± 0.02 | 
| 8. Molecular wt.(mn) | : | approx.3000 | 
KP-5065 is usually cross linked with HMM Melamine resins. The addition of HMMM is usually between 15
  – 30% on solid basis. Incorporation of acid catalyst e.g. Para toluene sulphonic acid promotes the curing.
  1% to 5% of acid catalyst on Melamine solids is recommended.
The product has excellent pigment wetting properties and high yield pigment concentrates can be formulated.
CURING SCHEDULES :| Coil Coating finishes based on KP-4060 can be cured using a peak metal temperature of 232°C - 240°C. For Metal Decorating, a cure schedule of 10 minutes at 160 -200°C depending on requirements is recommended; cure response will increase with temperature, but flexibility may be reduced with high levels of catalyst. For General Industrial applications a baking schedule of 30 minutes at 150°C will be suitable. | Metal Decorating: 72 : 18 : 10 KP-4060 Curing of 10 minutes at 160 - 200 is recommended. Aromatic hydrocarbons are recommended. | 
| General Industrial enamels: 70 : 30 to 80 : 20 on solids with hexamethoxymethyl melamine resin or partly methylated melamine with 2% PTSA catalyst on amino levels. Baking of 30 minutes at 150 C is recommended. Blend of aromatic hydrocarbon/ alcohol are suggested | 
Keep away from heat source & direct sunlight. Avoid temp.more than 30 degree C.
PACKING :210 kg. Net in new MS drums